夏季腻子粉施工不留神就会出现这些问题
来源://www.gochiism.com 日期:2023-07-17 发布人:
气温逐渐开始高升,已经进入了盛夏,小编整理了一些关于夏天批刮腻子粉容易出现的问题,看完之后记得要整理要点并规避起来。
The temperature is gradually starting to rise, and it has entered the peak of summer. The editor has compiled some questions about the problems that may occur when applying putty powder in batches in summer. After reading them, remember to organize the key points and avoid them.
1
one
干得快
dry fast
济南腻子粉粉料在桶里调配时干的很快,难施工,批刮后失水快,不能正常收压或施工后干燥过快。
Jinan putty powder dries quickly when mixed in barrels, making it difficult to construct. After scraping, it loses water quickly, and cannot be compressed properly or dried too quickly after construction.
原因:施工环境气温太高,湿度太低、通风太强及阳光直晒,腻子粉中的复合材料反应加速。
Reason: The temperature in the construction environment is too high, the humidity is too low, the ventilation is too strong, and the direct sunlight accelerates the reaction of the composite materials in the putty powder.
解决方案:预防为主,注意施工环境,避免在高温时段、阳光直晒时段施工,控制施工场地通风强度。当基面出现太过干燥、 吸水快的情况时建议刷涂界面剂或者预先湿润基面(但不能有明水)再施工。
Solution: Prevention first, pay attention to the construction environment, avoid construction during high temperature and direct sunlight periods, and control the ventilation intensity of the construction site. When the base surface becomes too dry or absorbs water quickly, it is recommended to brush the interface agent or wet the base surface in advance (but without clear water) before construction.
2
two
批刮翻卷、卷皮
Batch scraping, flipping, and peeling
腻子粉在批刮、收压时出现翘起或呈鳞片现象。
The putty powder shows tilting or scaling during batch scraping and pressing.
原因:基面太干燥或施工现场温度太高。
Reason: The base surface is too dry or the construction site temperature is too high.
解决方案:基层太干燥时应保湿施工,避开中午这种高温时段施工。而针对批刮已翻皮的腻子粉应该铲除腻子粉,重新批刮。
Solution: When the base layer is too dry, it should be moisturized during construction, avoiding high temperature periods such as noon. For the putty powder that has been peeled and scraped in batches, the putty powder should be removed and scraped again.
3
three
起泡
Bubbling
腻子粉批刮时产生气泡或者批刮过后表面起泡。
Bubbles are generated during the batch scraping of putty powder or the surface blisters after the batch scraping.
原因:夏季气温高, 基层过于干燥致使腻子粉快干,从而产生气泡。
Reason: In summer, the temperature is high, and the base layer is too dry, causing the putty powder to dry quickly, resulting in bubbles.
解决方案:腻子粉调配时应按要求充分搅拌,在适宜温度范围施工。如若批刮时腻子粉有气泡可在表干时反复收压,消除气泡。
Solution: When mixing putty powder, it should be thoroughly mixed as required and constructed within the appropriate temperature range. If there are bubbles in the putty powder during batch scraping, it can be repeatedly compressed while the surface is dry to eliminate the bubbles.
4
four
掉粉、脱层
Powder shedding and delamination
施工完成及干透后,用手触摸有掉粉现象,严重的甚至出现前后两道腻子粉之间或腻子粉与基底之间相互剥离。
After the construction is completed and dried thoroughly, there is a phenomenon of powder falling when touched by hand, and in severe cases, there may even be peeling between the two layers of putty powder or between the putty powder and the substrate.
原因:腻子粉在高温干燥时施工,水分挥发快,没有足够水分进行固化,因而容易脱粉。而底层腻子粉疏松粉化严重,面层腻子粉太硬,干燥太快会造成脱层。另外,外墙腻子粉被雨水冲刷后,粘结剂流失,重批后也容易脱层。
Reason: Putty powder is applied at high temperatures and dryness, causing rapid moisture evaporation and insufficient moisture for solidification, making it easy to peel off the powder. And the bottom layer putty powder is loose and severely powdery, while the surface layer putty powder is too hard and dries too quickly, which can cause delamination. In addition, after the external wall putty powder is washed away by rainwater, the adhesive is lost, and it is also easy to delaminate after re approval.
解决方案:腻子粉调配时应按要求充分搅拌,在适宜温度范围施工。如若批刮时腻子粉有气泡可在表干时反复收压,消除气泡。
Solution: When mixing putty powder, it should be thoroughly mixed as required and constructed within the appropriate temperature range. If there are bubbles in the putty powder during batch scraping, it can be repeatedly compressed while the surface is dry to eliminate the bubbles.
夏季,腻子粉应该注意防通风过强、防太阳直晒、防高温时段施工,注意了这些其实夏季也不失为一个批腻子粉的好季节。同时,高温季节施工,工人防中暑的工作也要做好。更多相关事项就来我们网站//www.gochiism.com咨询!
In summer, putty powder should be prevented from excessive ventilation, direct sunlight, and construction during high temperature periods. It should be noted that summer is actually a good season for putty powder batch. At the same time, during the hot season of construction, workers should also do a good job in preventing heatstroke. For more related matters, come to our website //www.gochiism.com consulting service