灌浆料使用不当时会容易出现的问题

来源://www.gochiism.com 日期:2023-03-16 发布人:

许多大型设备需要固定在高强度基面上才能运行,而混凝土结构其强度和抗疲劳性都达不到设备运行要求,这时我们就要用灌浆料对其进行加固。设备基础二次灌浆时如果忽略了一些小细节,其灌浆效果就会大打折扣。那么灌浆料使用不当时容易出现哪些问题呢?济南腻子粉厂家为您分析:
Many large equipment need to be fixed on the high-strength base surface to operate, and the strength and fatigue resistance of concrete structures can not meet the equipment operation requirements, so we need to use grouting materials to reinforce them. If some small details are omitted during the secondary grouting of equipment foundation, the grouting effect will be greatly reduced. What problems are likely to occur when grouting materials are not used properly? Jinan putty powder manufacturer analyzes for you:
一、基面处理不完全:灌浆料使用前,我们要对基面进行清理,清除基面上的油污、不易粘结的小颗粒、粉尘等,同时还要润湿基面,但不要留明水。倘若基面处理不干净,利用设备基础二次灌浆料施工时,就会导致粘结不牢固现象。
1、 Incomplete treatment of the base surface: before using the grouting material, we should clean the base surface, remove the oil dirt, small particles that are not easy to bind, dust, etc. on the base surface, and also wet the base surface, but do not leave open water. If the base surface is not cleaned, the bonding will not be firm when the secondary grouting material for equipment foundation is used for construction.
二、搅拌不均匀:在灌浆料施工时,我们要严格按照其水料比进行搅拌,同时搅拌时间、搅拌力度要充分,保障灌浆料搅拌均匀才能使用。搅拌不均匀的灌浆料会出现充盈度差,容易泌水,强度低,易开裂。
2、 Uneven mixing: during the construction of grouting materials, we should mix them in strict accordance with their water-material ratio, and at the same time, the mixing time and mixing strength should be sufficient to ensure that the grouting materials can be mixed evenly before use. Uneven mixing of grout will lead to poor filling, easy bleeding, low strength and easy cracking.
济南腻子粉
三、施工不连续:灌浆料在进行灌浆施工要连续,中途不能间隔太久,同时搅拌好的浆料要一次性使用完毕,若中途因流动度不够,不得加水,应当废弃。中途加水容易导致泌水,强度不均,开裂现象。
3、 Discontinuous construction: The grouting material shall be continuous during the grouting construction, and the interval shall not be too long. Meanwhile, the mixed grout shall be used at one time. If the fluidity is insufficient during the grouting construction, no water shall be added, and it shall be discarded. Adding water halfway can easily lead to bleeding, uneven strength and cracking.
四、施工方位不当:灌浆施工时我们应从一端向另一端进行,或者从中间向四周进行,以排出模板间的空气,防止气泡封存与浆料中,切忌为了赶速度从四周同时灌浆。
4、 Improper construction orientation: during grouting construction, we should carry out from one end to the other end, or from the middle to the four sides, so as to exhaust the air between the formwork and prevent bubbles from being sealed in the slurry, and we should not grout from the four sides at the same time in order to catch up.
五、养护不当或不养护:灌浆料施工完毕后,需进行养护7天左右,通常为洒水养护,保障表面处于湿润状态即可,温度处于零下时,还要进行保温。如不进行养护会影响灌浆料抗压强度等性能。
5、 Improper or no curing: After the completion of the grouting material construction, it needs to be cured for about 7 days, usually by sprinkling water to ensure that the surface is in a wet state. When the temperature is below zero, it also needs to be insulated. Without curing, the compressive strength and other properties of the grouting material will be affected.
灌浆料使用不当时会容易出现的问题相关内容就是以上所讲解到的,希望能够帮助到您,当然要注意一点,好的施工材料配合正确的施工方法才能取得理想的效果。您有不了解的地方欢迎来我们网站//www.gochiism.com留言咨询!
The relevant content of problems that may occur when grouting materials are not used properly is explained above. I hope it can help you. Of course, we should pay attention to that good construction materials and correct construction methods can achieve ideal results. Welcome to our website if you don't know anything //www.gochiism.com Message consultation!