腻子粉厂家介绍腻子粉的施工流程
来源://www.gochiism.com 日期:2021-09-30 发布人:
济南腻子粉的施工过程是怎样的?
What is the construction process of Jinan putty powder?
一.模子
1、 Mold
原因:
reason:
济南腻子粉厂家在墙地幕墙时,其原料是海藻和水泥的混合物,其酸碱度较高,因此踢脚也比较容易,它会与p反应对湿线和带有壁泄漏的区域进行反应。这种现象会导致壁上的翅膀,发霉并剥落皮肤。
When Jinan putty powder manufacturer is in the wall and ground curtain wall, its raw material is the mixture of seaweed and cement. Its pH is high, so it is easy to skirting. It will react with P to react with the wet line and the area with wall leakage. This phenomenon can cause the wings on the wall to become moldy and peel off the skin.
加工方式:
Processing method:
可以干净地除去发霉的无壳壁,并可以清洗干净的水,并且如果泄漏或潮湿的壁可以立即关闭水源,并且可以在壁干燥后再次去除碱性粉末。
The moldy shell free wall can be removed cleanly, and the clean water can be cleaned. If the wall is leaked or wet, the water source can be turned off immediately, and the alkaline powder can be removed again after the wall is dry.
注意:通常,墙壁发霉,春季天气基本炎热。
Note: usually, the walls are moldy, and the weather is basically hot in spring.
二.做快点
2、 Do it quickly
原因:
reason:
1.由于夏季天气相对炎热,水的蒸发相对较快,而在批量除尘工作中水的挥发相对较快。出现的比路还多。
1. Due to the relatively hot weather in summer, the evaporation of water is relatively fast, while the evaporation of water in batch dust removal is relatively fast. There are more than roads.
2.生产原因:发生速干现象的原因是生产商无意中误认为原料的混合比例,或者由于设备异常而使混合变得不稳定。
2. Production reasons: the reason for the quick drying phenomenon is that the manufacturer inadvertently mistook the mixing proportion of raw materials, or the mixing became unstable due to abnormal equipment.
加工方式:
Processing method:
1.施工时的天气为35°C,在稀薄的鼓风机和物料搅拌下,接下来的两种或多种腻子粉的使用方法很少。
1. The weather during construction is 35 ° C. under the mixing of thin blower and materials, the next two or more putty powders are rarely used.
2.出现速干现象时,济南腻子粉厂家工程师会到现场,根据产品的配方判断是否速干。
2. In case of quick drying, the engineer of Jinan putty powder manufacturer will come to the site to judge whether it is quick drying according to the product formula.
注意:如果出现速干现象,则可以像之前一样在进行约2小时的表面干燥后立即进行下一次构造,从而减少速干。
Note: if rapid drying occurs, the next construction can be carried out immediately after about 2 hours of surface drying as before, so as to reduce rapid drying.
三.针孔
3、 Pinhole
原因:
reason:
1.正常现象是在一批时出现针孔。在一批的情况下,粉末层厚且难以弄平,这影响了在弄平后第2条的粘合力。针孔通常在墙壁相对不平坦的一些道路上形成,但由于针孔吃掉了大量材料,针孔会缓慢干燥,并且经纱上铺有凹陷的粉末。由于困难,所以发生针孔现象。
1. The normal phenomenon is pinholes in a batch. In the case of a batch, the powder layer is thick and difficult to flatten, which affects the adhesion of Article 2 after flattening. Pinholes are usually formed on some roads with relatively uneven walls, but because the pinholes eat a lot of material, the pinholes will dry slowly, and the warp yarn is covered with concave powder. Pinholes occur due to difficulties.
腻子粉厂家
Putty powder manufacturer
2.由于施工过程中光线不足,济南腻子粉厂家施工人员在施工过程中会忽略墙面上的小针孔,因而无法及时接收,从而造成针孔现象。
2. Due to the lack of light during construction, the construction personnel of Jinan putty powder manufacturer will ignore the small pinholes on the wall during construction, so they cannot receive them in time, resulting in pinholes.
加工方式:
Processing method:
1.对于不平坦的墙壁,在一个施工过程中必须使平面尽可能平整。
1. For uneven walls, the plane must be as flat as possible during a construction process.
2.施工时要小心,天气不好时光线不足,或者晚上天黑时,要在腋下用照明设备进行施工,济南腻子粉厂家会避免施工错误,要用人造针进行施工避免孔洞问题。
2. Be careful during construction. When the weather is bad, the time line is insufficient, or it is dark at night, the construction shall be carried out with lighting equipment under the armpit. Jinan putty powder manufacturer will avoid construction errors and use artificial needles to avoid hole problems.
如果腻子粉的粉末太粘或太慢,可能会出现针孔,因此必须注意产品配方的合理性。
If the powder of putty powder is too sticky or too slow, pinholes may appear, so we must pay attention to the rationality of the product formula.