腻子层掉粉变黄是怎么回事?
来源://www.gochiism.com 日期:2019-08-13 发布人:
腻子层掉粉变黄是怎么回事?
What's the matter of putty powder dropping and yellowing?
一、腻子上一层粉
1. A layer of powder on the putty
落粉原因:
Reasons for flour drop:
1. 腻子粉的牌子不够好。腻子粉的抛光时间不够好。
1. Putty powder is not good enough. The polishing time of putty powder is not good enough.
2. 产品超过保质期,粘接强度大大降低。
2. When the product exceeds the shelf life, the bonding strength decreases greatly.
3、产品贮存不当,吸湿后粘接力明显减少。
3. The adhesive force of the product decreased obviously after hygroscopicity due to improper storage.
4、基材吸水率高,导致腻子干燥速度快,没有足够的水进行固化。
4. The high water absorption of the base material results in the fast drying speed of putty and insufficient water for curing.
滴粉溶液:
Dropping powder solution:
1、内墙腻子表面层抛光要掌握合适的抛光时间,抛光的佳时间是等待腻子表面水印消失后,立即抛光。
1. Proper polishing time should be mastered in polishing the surface layer of putty on the inner wall. The best polishing time is to wait for the putty surface watermarking to disappear and polish immediately.
腻子粉
Putty powder
2. 产品必须在保质期内使用。如果超过保质期,必须进行测试和刮擦。在建设。
2. Products must be used within the shelf life. If it exceeds the shelf life, it must be tested and scraped. Construction is under way.
3、产品必须注意防水,应放在阴凉干燥处,并确保包装完好。
3. The product must be waterproof, should be placed in a cool and dry place, and ensure that the packaging is in good condition.
4、夏季或高温气候条件下,敷吹风机腻子前好先用清水湿润墙面,墙面表面没有清水后,可敷吹风机腻子。
4. In summer or high temperature climatic conditions, it is better to wet the wall with clear water before applying the putty. If there is no clear water on the wall surface, the putty can be applied.
5、购买知名腻子粉品牌。
5. Buy well-known putty powder brand.
2. 腻子层变黄了
2. Putty layer yellows
1、与聚酯漆(涂料)或脱模剂同时使用,造成腻子膜发黄。
1. Use with polyester paint (paint) or release agent at the same time, resulting in putty film yellowing.
2、底座有油脂或其他油脂污垢,未清理干净,导致腻子膜发黄。
2. There is grease or other grease dirt on the base, which is not cleaned up, resulting in yellowing of putty membrane.
3.腻子膜受锈蚀或其它死物料污染,可能导致腻子膜发黄。
3. Putty membranes are contaminated by rust or other dead materials, which may cause putty membranes to yellowish.
4. 腻子粉的品牌。
4. Putty powder brand.
泛黄的解决方案:
Solutions to yellowing:
避免与聚酯漆(漆)或脱模剂同时使用。
Avoid using with polyester paint or release agent.
2. 底座应清洗干净,避免油渍。
2. The base should be cleaned to avoid oil stains.
3、腻子施工后,注意成品的保护,避免污染。
3. After putty construction, pay attention to the protection of finished products to avoid pollution.
4. 施工温度不宜过低或低于5度。
4. Construction temperature should not be too low or below 5 degrees.
5、购买有保证的腻子粉品牌。