腻子粉施工完毕后出现针孔的原因
来源://www.gochiism.com 日期:2022-10-18 发布人:
济南腻子粉在进行施工前后如果不认真仔细就会出现一些问题,让整个工程项目质量受到影响,比如腻子粉施工完毕后出现针孔,下面济南腻子粉厂家为您解析。
If Jinan putty powder is not careful before and after construction, some problems will occur, which will affect the quality of the whole project. For example, pinholes will appear after the putty powder construction is completed. Now, Jinan putty powder manufacturer will analyze for you.
产生原因:
Cause:
1、批刮一道时出现针孔属于正常现象。因为一道在批刮时腻子粉层较厚,且不宜收平,收太平以后将会影响二道得附着力。二,三道出现针孔得一般会是一些墙面较为凹凸不平得地方,由于凹凸不平得地方吃料比较多,比较慢干,刮刀较难将凹得地方腻子粉层压实,因而会产生一些针孔现象。
1. It is normal to have pinholes when scraping once. Because the putty powder layer of the first layer is thick and should not be leveled, the adhesion of the second layer will be affected after leveling. 2、 The three pinholes are usually the uneven places on the wall. Because there are many materials in the uneven places, which dry slowly, it is difficult for the scraper to compact the putty powder layer in the concave places, so there will be some pinholes.
2、由于施工时光线不足会导致施工人员在施工时对墙面上一些较为小得针孔忽略,未及时收平而导致得一些针孔现象。
2. Due to the lack of time line during construction, the construction personnel will ignore some small pinholes on the wall during construction, and they will not be leveled in time, resulting in some pinholes.
处理方法:
Handling method:
1.关于高低不平的墙面应该在一道腻子粉批刮施工时应尽量补平(因为一道发生纤细的针孔不会影响二道的正常施工)这样有利于批刮二,三道腻子粉层时收平,削减针孔的发生。
1. The uneven wall surface should be filled as much as possible when one layer of putty powder is applied (because the fine pinholes in one layer will not affect the normal construction of the second layer), which is conducive to the application of two layers of putty powder and the leveling of three layers of putty powder to reduce the occurrence of pinholes.
2.腻子粉在批刮施工时应注重光线,如遇气候欠好时光线缺乏或黄昏时光线由亮转暗时,应在有照明设备的帮肋下进行施工,避免因施工失误而构成人为的针孔疑问。
2. Pay attention to the light when applying putty powder. If the weather is bad and the time line is short or the time line changes from light to dark at dusk, the putty powder shall be applied under the rib of the lighting equipment to avoid man-made pinhole problems caused by construction mistakes.
此外要注意腻子粉粘度较高或比较慢干也会产生一些针孔现象,应注意产品配方得合理性。关注我们//www.gochiism.com,带您了解更多产品事项!
In addition, it should be noted that higher viscosity or slower drying of putty powder will also cause some pinholes, and the product formula should be reasonable. Follow us //www.gochiism.com , take you to know more about products!